Origin:Made In Taiwan

Material :Polyester

Specification :DTY 110±10D/36F

Strength :2g/d

Elongation :25±10%

Luminous intensity :≧ 40-50 mcd/g-m2

Color type :White yarn could be green light or blue light

Identity :The light from the LUMI LONG TM luminous fiber can stable emit 6 hours by absorbing surrounding light for 10 minutes without any extra electricity and the heat and radiation were not detected.

The ultra-soft phosphorescent elasticity knitted cloth is created by advanced knitting technology.
This cloth has softness, rewash able, and steam iron able properties

 

 

Fiber Safety qualification

1.Atomic Energy Council, Executive Yuan 
   (Reference number : 1001231 )
2.Taiwan Toy Research &. Development Center (TTRD) 
   Evaluation of free formaldehyde emission (Reference number : 10006142CSF497-2)
3.SGS 
   Without migration fluorescent, Heavy metals, Carcinogenic dyes, Phthalate
   (Reference number : TXN1476A/2011/SH)

 

Analysis of Luminous fiber

  From the photograph of scanning electron microscope (SEM) for different luminous fiber, the Lumilong fiber has not only a special sheath/core structure but also a smooth fiber surface without any particle adhesion. According to the competition product, the SEM photograph shows a rough surface and the particle almost disappear after fiber washing test and the fiber luminous intensity approach to 0. The results show that luminous fiber from surface coating or doped dye yarn cannot sustained the washing test, the detached of luminous particle could be easily harmful for human skin and knitting machine .

 

 

Analysis of fiber luminous intensity

1. Sample preparation :
    According to the standard method of ASTM D1907-89, the length of sample fiber were repared 90 meters by winding machine and the weight of fiber was recorded. Each step were tested for three times in order to check the data repeatability.


2. Evaluation of fiber luminous intensity :
    The sample testing atmosphere was controlled at 25±2℃, humidity around 65±10ï¼…RH, the D65 lamp with 1100±50Lux was prepared to light to fiber sample for 10 minutes. The results was analyzed by Klein Instruments color meter .

 

The results of fiber analysis

    According to the standard method of AATCC135-2010, WOB cleaning agent without fluorescent whitening agent were selected, the dosage of cleaning agent was controlled to 66±1g, the washing temperature and washing time were also controlled at 41±3℃ and 12 minutes. After washing step, the samples were drying at 60±5℃ for 45minutes and cooling at room temperature for 10minutes. The 1 cycle of fiber washing testing was also accomplished.

LUMI1223

LUMI1223

Composition:100%polyester WIDTH:61" WEIGHT:249g/y

LUMI1223

LUMI1223

Composition:100%polyester WIDTH:61" WEIGHT:249g/y

LUMI1224

LUMI1224

97%polyester 3%spandex WIDTH:60" WEIGHT:247g/y 174g/m^2

LUMI1224

LUMI1224

97%polyester 3%spandex WIDTH:60" WEIGHT:247g/y 174g/m^2

LUMI1225

LUMI1225

97%polyester 3%spandex WIDTH:61" WEIGHT:249g/y

P1140231.JPG

P1140231.JPG

LUMI1213

LUMI1213

Composition:100%polyester WIDTH:60" WEIGHT:240g/y

LUMI1213

LUMI1213

Composition:100%polyester WIDTH:60" WEIGHT:240g/y

LUMI1220

LUMI1220

Composition:97%polyester 3%Spandex WIDTH:60" WEIGHT:250g/y

LUMI1220

LUMI1220

Composition:97%polyester 3%Spandex WIDTH:60" WEIGHT:250g/y

LUMI1221

LUMI1221

Composition:97%polyester 3%Spandex WIDTH:62" WEIGHT:210g/y

LUMI1221

LUMI1221

Composition:97%polyester 3%Spandex WIDTH:62" WEIGHT:210g/y

The results of fiber analysis

The results of fiber analysis

The results of fiber analysis According to the standard method of AATCC135-2010, WOB cleaning agent without fluorescent whitening agent were selected, the dosage of cleaning agent was controlled to 66±1g, the washing temperature and washing time were also controlled at 41±3℃ and 12 minutes. After washing step, the samples were drying at 60±5℃ for 45minutes and cooling at room temperature for 10minutes. The 1 cycle of fiber washing testing was also accomplished.

SEM

SEM

Analysis of Luminous fiber From the photograph of scanning electron microscope (SEM) for different luminous fiber, the Lumilong fiber has not only a special sheath/core structure but also a smooth fiber surface without any particle adhesion. According to the competition product, the SEM photograph shows a rough surface and the particle almost disappear after fiber washing test and the fiber luminous intensity approach to 0. The results show that luminous fiber from surface coating or doped dye

Analysis of fiber luminous intensity

Analysis of fiber luminous intensity

1. Sample preparation : According to the standard method of ASTM D1907-89, the length of sample fiber were repared 90 meters by winding machine and the weight of fiber was recorded. Each step were tested for three times in order to check the data repeatability. 2. Evaluation of fiber luminous intensity : The sample testing atmosphere was controlled at 25±2℃, humidity around 65±10%RH, the D65 lamp with 1100±50Lux was prepared to light to fiber sample for 10 minutes. The results was analy

  • facebook
  • Twitter Clean
  • w-googleplus

2013 SHUAN JIUH Workshop.
All rights reserved.

Visit

335  Touliao, Daxi Township,Taoyuan County 335, Taiwan (R.O.C.)

 

Call

T:886-3-387-1059 

   886-3-387-0589

   070-1000-1789
F: 886-3-387-0569

bottom of page